MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® WR-9750 Extrusion Grade ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM D792
Melt Flow 3.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785
Tensile Strength at Break 5700 psiASTM D638
Elongation at Break 80 %ASTM D638
Flexural Strength 7800 psiASTM D790
Flexural Modulus 241000 psiASTM D790
Izod Impact, Notched 11.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 187 °F
@Thickness 6.35 mm
Unannealed; ASTM D648
Vicat Softening Point 95.0 °CISO R-306
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 374 - 410 °FH1
Middle Barrel Temperature 410 - 446 °FH2
Front Barrel Temperature 428 - 464 °FH3
Nozzle Temperature 428 - 464 °F
Mold Temperature 104 - 176 °F
Drying Temperature 176 °F
Dry Time 2 - 4 hour
Injection Pressure 9900 - 21300 psi
Back Pressure 142 - 284 psi
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® WR-9140 General Purpose ASA
A. Schulman Diamond ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned
LG Chemical LI-941 ASA, Extrusion, High Heat Resistance
LG Chemical LI968W Co-Extrusion ASA

PLBST109 / 50494

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.