MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Superwool® Blok Plus 1000 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® Plus Blok sheets are made from Superwool ® Plus fibers, mineral fibers and a small amount of organic binder. Due to the high fiber content, Superwool ® Plus Blok sheets are strong, lightweight and thermal shock resistant. All grades of Superwool ® Plus Blok receive a water repellence treatment to prevent absorption of water or concrete binders. The panels must be installed so that the side with the product name is in contact with the concrete. When tested on this side, Superwool ® Plus Blok is classified as non hydrophilic (NF P 75-305).

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000800 GPa0.116 ksi
Compressive Strength 0.400 MPa58.0 psiat 5% reduction in thickness
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0600 W/m-K
@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 392 °F
ASTM C-201
 0.0600 W/m-K
@Temperature 300 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 572 °F
ASTM C-201
 0.0700 W/m-K
@Temperature 400 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-201
 0.0900 W/m-K
@Temperature 500 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 932 °F
ASTM C-201
 0.100 W/m-K
@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-201
 0.110 W/m-K
@Temperature 700 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1290 °F
ASTM C-201
 0.130 W/m-K
@Temperature 800 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-201
 0.160 W/m-K
@Temperature 900 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1650 °F
ASTM C-201
Maximum Service Temperature, Air 1000 °C1830 °F
Shrinkage 1.6 %
@Time 86400 sec
1.6 %
@Time 24.0 hour
isothermal heating @ classification temp; ENV-1094-1
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 5.5 %5.5 %
 
Descriptive Properties
Classification Temperature (°C)1100
Colorwhite
Water Absorption (kg/m3)5NF-P75-302, after 96 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF7031 / 203330

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.