MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Lankropol 4500 Dioctyl Sodium Sulfosuccinate in ethanol/water
Categories: Other Engineering Material

Material Notes: Sodium di-(2-EH) sulfosuccinate in ethanol/water.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Solids Content 70 %70 %
pH 5.0 - 7.05.0 - 7.01% in water
Surface Tension 26.3 dynes/cm26.3 dynes/cmaccording to Du Noüy at 0.05% solids solution at 25°C
 
Chemical PropertiesMetricEnglishComments
Acid Value 3.03.0[mg KOH/g]
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 19 - 24 %19 - 24 %
 
Descriptive Properties
AppearanceClear to slightly hazy liquid
Color0-35Platinum Cobalt
 35APHA
Content0-0.05Sodium Sulfite
 216 ppmCalcium Tolerance, CaCo3 at 0.25% solids in water
 68-72 %Solid content
Content (%)70Active content
Wetting power10 secDraves, at 0.035% solids in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY598 / 286121

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.