MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound MFD03 Polypropylene, Unspecified (PP, Unspecified) (Americas)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP STAT-KON MFD03 compound is based on Polypropylene (PP) resin containing conductive carbon powder and 15% glass fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
 1.07 g/cc0.0387 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/in24hrs; ASTM D955
 0.010 cm/cm0.010 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in24hrs; ASTM D955
 0.0092 cm/cm0.0092 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.0 MPa2180 psiISO 527
 16.0 MPa2320 psiASTM D638
Tensile Strength, Yield 34.0 MPa4930 psiASTM D638
 34.0 MPa4930 psiISO 527
Elongation at Break 5.7 %5.7 %ISO 527
 6.9 %6.9 %ASTM D638
Elongation at Yield 2.6 %2.6 %ISO 527
 2.7 %2.7 %ASTM D638
Tensile Modulus 3.31 GPa480 ksi1 mm/min; ISO 527
 3.44 GPa499 ksi50 mm/min; ASTM D638
Flexural Strength 51.0 MPa7400 psiISO 178
Flexural Modulus 2.75 GPa399 ksiASTM D790
 3.00 GPa435 ksiISO 178
Izod Impact Notched 347 J256 ft-lbASTM D256
Izod Impact, Unnotched 1.38 J/cm2.59 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 J9.59 ft-lbpeak; ASTM D3763
Impact Test 5.00 J3.69 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 - 1.00e+6 ohm1000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  46.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
26.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 47.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
26.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  104 µm/m-°C
@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 147 °C
@Thickness 3.20 mm
297 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 106 °C
@Thickness 3.20 mm
223 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 215 - 225 °C419 - 437 °F
Zone 3 240 - 250 °C464 - 482 °F
Melt Temperature 225 - 250 °C437 - 482 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81323 / 289270

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.