This product is a one-component polyurethane, 100% solids, reactive hot melt adhesive. Features and Benefits: - Thermal and solvent resistance
- Good low temperature flexibility
- Excellent abrasion resistance
- High modulus/high impact strength
- Designed for fast automated lines and hot plant temps
- Very high green strength