MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem Weston™ TLP Antioxidant
Categories: Other Engineering Material

Material Notes: Product Description: Weston™ TLP phosphite ester is a trialkyl phosphite which can be used as a lubricant additive to improve antifriction and antiwear characteristics. It also functions as a sulfur deactivator. Weston™ TLP phosphite ester may be used as a stabilizer in PVC polyester fibers and in polypropylene when regulatory approval for food contact is not required.

CAS No: 25550-98-5

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.866 - 0.881 g/cc0.866 - 0.881 g/cc
Viscosity 16 cP
@Temperature 37.8 °C
16 cP
@Temperature 100 °F
Molecular Weight 586 g/mol586 g/mol
Vapor Pressure 0.00667 bar
@Temperature 190 °C
5.00 torr
@Temperature 374 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.050<= 0.050[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 166 °C330 °FPensky-Martens Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.453 - 1.4581.453 - 1.458
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 5.3 %5.3 %
 
Descriptive Properties
AppearanceClear liquid
Color<50APHA, Pt/Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH518 / 315436

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.