MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt Silvally® 45 Flux Coated Rod Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 45 FC is the lowest melting brazing alloy available composed of silver, copper, zinc, and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It has a wide acceptance by industrial users, as well as being included in Federal military specifications on brazing filler metals or alloys. It has a narrow melting range which is not apparent in most brazing operations, making it flow freely though a capillary. Typical applications are the joining of ferrous, non-ferrous, and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: AWS BAg-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 9.34 g/cc9.34 g/cc
Density 9.41 g/cc0.340 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000606 ohm-cm0.00000606 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 607.2 - 618.3 °C1125 - 1145 °F
Solidus 607.2 °C1125 °F
Liquidus 618.3 °C1145 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 618.3 - 760 °C1145 - 1400 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 13.93 - 15.93 %13.93 - 15.93 %
Copper, Cu 4.33 - 14.33 %4.33 - 14.33 %As balance of metal
Silver, Ag 27 - 29 %27 - 29 %
Zinc, Zn 7.96 - 11.96 %7.96 - 11.96 %
 
Descriptive Properties
Boric Acid %0-30percentage of flux
ColorLight Yellow
Colored Pigments %0-0.05percentage of flux
Electrical Conductivity (% IACS)27.6
Flux36.78-38.78%
Potassium Bifluoride %0-30percentage of flux
Potassium Fluoroborate %0-30percentage of flux
Potassium Pentaborate %1-5.0percentage of flux
Potassium Tetraborate %0-40percentage of flux
Sodium Dodecyl Sulfate %0-0.5percentage of flux

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy
Lucas-Milhaupt Silvaloy® 501 Brazing Alloy
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy
Lucas-Milhaupt Silvaloy® 45 Brazing Alloy
Lucas-Milhaupt Silvaloy® 402 Brazing Alloy

NBRW031 / 79807

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.