MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Apcotex Apcotex SR 568 High Styrene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Key Advantages:
  • Contains non-staining antioxidant
  • Very high Styrene Content
  • Can impart very high Hardness
  • Very good Flex Resistance
  • Very Good Abrasion Properties
  • Improves surface finish & flex fatigue when used to reinforce elastomers
  • Can be Moulded as well as Extruded.
Applications:
  • Highly suitable for Hawaii soles and Microcellular sheets
  • Finds applications in Automotive and Industrial Goods
  • Also used to improve Hardness and Gloss in various rubber compounds
  • Reinforcement of natural and many synthetic rubbers (SBR, NBR, EPDM, EVA)

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
Volatiles <= 2.0 %
Mooney Viscosity 40 - 65
@Temperature 100 °C
ML 1+4
Ash <= 0.50 %
Storage Temperature <= 35.0 °C
 
Chemical PropertiesOriginal ValueComments
Styrene Content 68 %Bound
 
Processing PropertiesOriginal ValueComments
Shelf Life <= 24.0 Month
 
Descriptive Properties
AppearanceLight Tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPCOT023 / 315602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.