MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Die Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Used in bearing applications. ZA-12 has a higher bearing load capacity than bronze bearing alloys, although its environment (both temperature and corrosive) is more limited.

Key Words: UNS Z35630 (ingot); UNS Z35631 (Casting); ZA-12 Zinc Foundry Alloy; Previously ILZRO 12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 100500 kg load; 10 mm hardened steel ball
Hardness, Knoop 125Estimated from Brinell Value
Hardness, Rockwell A 41.5Estimated from Brinell Value
Hardness, Rockwell B 63Estimated from Brinell Value
Hardness, Vickers 112Estimated from Brinell Value
Tensile Strength, Ultimate 404 MPa
Tensile Strength, Yield 320 MPa
@Strain 0.2 %
Elongation at Break 5.0 %in 5 cm
Modulus of Elasticity 83.0 GPa
Compressive Strength 269 MPa
Fatigue Strength 117 MPa
@# of Cycles 5.00e+8
Reverse Bend
Fracture Toughness 14.4 MPa-m½
Shear Strength 296 MPa
Charpy Impact, Unnotched 12.0 J
@Thickness 6.35 mm
square bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 118 J/g
CTE, linear 24.1 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.450 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 116 W/m-K
Melting Point 377 - 432 °C
Solidus 377 °C
Liquidus 432 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 460 - 490 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10.5 - 11.5 %Addition, Casting
 10.8 - 11.5 %Addition, Ingot form
Cadmium, Cd <= 0.0050 %Impurity, Ingot form
 <= 0.0060 %Impurity, Casting
Copper, Cu 0.50 - 1.2 %Addition, Casting
 0.50 - 1.2 %Addition, Ingot form
Iron, Fe <= 0.065 %Impurity, Ingot form
 <= 0.075 %Impurity, Casting
Lead, Pb <= 0.0050 %Impurity, Ingot form
 <= 0.0060 %Impurity, Casting
Magnesium, Mg 0.015 - 0.030 %Addition, Casting
 0.020 - 0.030 %Addition, Ingot form
Tin, Sn <= 0.0020 %Impurity, Ingot form
 <= 0.0030 %Impurity, Casting
Zinc, Zn 87.193 - 88.68 %As balance; Ingot per ASTM B 669
 87.18 - 88.985 %As balance; Castings per ASTM B 791
 
Descriptive Properties
Damping5.1 Q-1 x 103at 100 Hz, 20°C
 9.8 Q-1 x 103at 100 Hz, 100°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast
Aluminum 6061-T6; 6061-T651
Zinc ILZRO 16 (Zn-1.25Cu-0.2Ti-0.15Cr), Die Cast
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast

MZN12C / 14518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.