MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Industeel SUPERELSO® 500 Quenched and Tempered High Strength Steel for Pressure Equipment
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: Superelso® 500 (SE 500) is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment. SE 500 is manufactured via the electric furnace with dephosphorisation, ladle refining and vacuum degassing to provide a reproducible, clean and homogeneous steel. The chemistry of SE 500 has been carefully adapted to combine high strength and excellent weldability. This steel also displays excellent toughness, with transition temperatures typically below -50°C/-58°F. This steel is particularly suitable for pressure equipment in the offshore oil and gas industry, where its high strength allows significant weight and cost reductions. It can be supplied with stainless steel or alloy cladding where necessary.

Mechanical properties for 150 mm plates or thinner.

Information provided by manufacturer.

Key Words: EN10028 part 6 P500QL2, ASTM A 533C Cl. 2 (mod.), ASME II Part A SA 533C Cl. 2 (mod.)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 600 - 720 MPa87000 - 104000 psiTypical
Tensile Strength, Yield >= 500 MPa
@Strain 0.2 %
>= 72500 psi
@Strain 0.2 %
Elongation at Break 18 %18 %Typical
Charpy Impact >= 50.0 J
@Temperature >=-50.0 °C
>= 36.9 ft-lb
@Temperature >=-58.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.13 %<= 0.13 %
Iron, Fe 96.356 - 100 %96.356 - 100 %As remainder
Manganese, Mn <= 1.6 %<= 1.6 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.0040 %<= 0.0040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A284 Steel, grade C
ASTM A284 Steel, grade D
Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service
Industeel SUPERELSO® 690CR Quenched and Tempered High Strength Steel for Leg Components of Jack-up Rigs
Latrobe LSS™ 135M Nitriding Steel (ASTM A355 Class A)

NINDUST62 / 17600

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.