MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Konson Accelerator ZnO-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% Finely selected zinc oxide, 20% EPDM/EVA binder and dispersing agents

Use Characteristics: Konson® ZnO-80 is a special grade of zinc oxide particularly suitable for the rubber industry. Due to its EPDM elastomer bound form, the absorption of humidity from the atmosphere during storage is prevented. In comparison to extrusion compounds containing powdered zinc oxide, those with Konson® ZnO-80 provide smoother profiles. This is due to the more homogeneous dispersion of Konson® ZnO-80. A slight increase in modulus and tensile strenghth usually occurs; elongation at break is also improved. Konson® ZnO-80 prevents the heat swell which normally occurs when powdered zinc oxide is used in CR mixes

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective ZnO is assured.

Dosage levels: 3 – 8 phr

Applications: Curing activator, particulary in the presence of fatty acids for almost kinds of rubbers.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.97 g/cc0.107 lb/in³
Loss On Ignition <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 195 - 200 °C383 - 392 °F
 
Descriptive Properties
AppearanceWhite to yellowish granules
Content= 99.8%ZnO
Sieve residue= 0.1 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS003 / 256048

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.