MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech Litho SP-2090 Polystyrene Sheet
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Description: Polystyrene Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 63ASTM D785
Tensile Strength, Yield 3300 psiASTM D638
Tensile Modulus 240000 psiASTM D638
Flexural Yield Strength 5800 psiASTM D790
Flexural Modulus 225000 psiASTM D790
Izod Impact, Unnotched 1.50 ft-lb/inASTM D256
Falling Dart Impact 460 ft-lb73°F; NBS PS-31-70
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 185 °FASTM D648
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Gloss 15 %Gardner; ASTM D2523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolan® 6050 Polystyrene, Injection Grade
INEOS Styrolution PS 165 N/L GPPS
American Polymers API 375 Polystyrene
A. Schulman Diamond GPPS BEADS Injection Molding Grade, General Purpose Polystyrene
Ineos Nova 2114 High Impact Polystyrene Extrusion Grade

PSPAR018 / 68459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.