MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Innospec VISCOWAX® 252 Oxidised PE-Wax
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: CAS Number: 68441 - 17 - 8

VISCOWAX® 252 – high quality oxidised, polar polyethylene wax.

Application:

  • Plastic processing
    • Lubricant for PVC
  • Paraffin compounding, candle industry
    • Increase on solidification and drop points
Applications as water-based Emulsions:
  • Textile Industry
    • Plasticizer component
    • Improvement of cross-linking properties, tear resistance and smoothing of fabrics
    • Slip agent for sewing threads
  • Paper industry
    • For surface finishing
  • Printing Inks
    • As anti-blocking / slip agent
    • Agent for abrasion prevention in aqueous printing inks
  • Die-casting industry
    • As release agent
  • Fruit coating

Information provided by Innospec Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 - 0.960 g/cc0.0340 - 0.0347 lb/in³DIN EN ISO 1183, C
Viscosity 150 - 300 cP
@Temperature 140 °C
150 - 300 cP
@Temperature 284 °F
DGF M-III 8
Molecular Weight 1700 g/mol1700 g/molGPC
 
Chemical PropertiesMetricEnglishComments
Acid Value 14 - 1814 - 18[mg KOH/g]; DGF M-IV 2
 
Mechanical PropertiesMetricEnglishComments
Penetration <= 3.0<= 3.0[10-1 mm], Needle; DGF M-III 9b
 
Thermal PropertiesMetricEnglishComments
Solidus 94.0 - 98.0 °C201 - 208 °FDGF M-III 4a
Dropping Point 102 - 108 °C216 - 226 °FDGF M-III 3
 
Descriptive Properties
AppearanceWhite-yellowish
Saponification value>30 mg KOH/gDGF M-IV 2
Type of deliveryFine grain

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® E-14EP Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer

PINOS024 / 183467

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.