MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds Mold Max® Stroke® Brushable Tin Catalyzed Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Mold Max™ STROKE™ is a brushable tin silicone rubber that self-thickens for making fast brush-on molds of almost any model. Properly applied, it will hold a vertical surface and will reproduce the finest detail. Mixed 100A:10B by weight, rubber quickly develops thixotropy and can be applied with a brush or spatula. Working time is 30 - 45 minutes with a re-coat time of 60 - 90 minutes depending on relative humidity. Cure time after the final layer has been applied is 16 hours at room temperature. Mold Max™ STROKE™ silicone will not stick to most surfaces and will cure with negligible shrinkage to a strong, flexible Shore 30A rubber. 4 thin layers is all that is necessary to make a strong and durable production mold for casting wax, gypsum, concrete or resins (urethane, polyester, etc.). Applications include reproducing sculpture, architectural restoration, candle molds, etc. Important; you must weigh Part A & B components using a gram scale to be successful with Mold Max™ STROKE™.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D-1475
Linear Mold Shrinkage 0.0020 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30ASTM D-2240
Tensile Strength 577 psiASTM D-412
Elongation at Break 300 %ASTM D-412
Tear Strength 125 pliDie B; ASTM D-624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 205 °C
Minimum Service Temperature, Air -53.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hour
 60.0 - 90.0 minRecoat Time
Pot Life 30.0 - 45.0 minASTM D-2471
 
Descriptive Properties
ColorWhite
Mix Ratio100A:10Bby weight
Mixed ViscosityBrushable
Specific Volume23.5[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN108 / 296809

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.