MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
NAECO® ELKONIUM® 40 pure palladium
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy; Pure Element

Material Notes: Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400°C. It has a high melting point (1552(C) and, like platinum, resists arc formation. Its low electrical conductivity (16% IACS) limits its application to low current circuits. It costs much less than platinum, and is used as a lower cost alternative. Economics normally dictate that it be supplied as a composite contact with a thin contact metal facing silver brazed to a nickel-plated steel rivet, screw, or projection weld button backing.

ELKONIUM® 40 is CMW's trademark for commercially pure palladium (9.90 minimum purity). Its good corrosion resistance and low hardness makes it a desirable contact for low current applications where forces are relatively low and reliability of making circuit is important. It is used in aircraft relays at currents under 1 ampere, in telephone relays and in instruments. It is often chosen for applications where contacts area open for long periods of time.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 15T 57annealed
 82cold worked
Tensile Strength, Ultimate 28000 psiannealed
 47000 psicold worked
Elongation at Break 5.0 %cold worked
 28 %annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000108 ohm-cm16 % IACS
 
Component Elements PropertiesOriginal ValueComments
Palladium, Pd >= 99.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2060602D1 Membrane Touch Switch Paste
NAECO® ELKONIUM® 42 palladium based alloy
NAECO® ELKONIUM® 41 palladium based alloy

NCMV906 / 192387

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.