MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total PPC 4824WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent antistatic properties.

Application

ATOFINA 4824WZ has been developed for high speed injection molding of thin-walled packaging containers and household articles.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 40 g/10 min40 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.5 MPa3700 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 1.17 GPa170 ksiASTM D 790
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256
 0.440 J/cm
@Temperature -20.0 °C
0.824 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²Notched/Unnotched not specified; ASTM DIN53453
 0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648
Vicat Softening Point 148 °C298 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin
Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
LyondellBasell Pro-fax™ SC973 Polypropylene Copolymer
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer

PFINAA073 / 38509

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.