MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

IDI Composites B30 BMC Thermoset Polyester, 20% Glass Fiber
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Low Profile Automotive Grade. Designed for applications that require a cost effective composite solution that possesses good dimensional stability and can accommodate tight tolerances. Possesses very low shrink characteristics and is well suited for applications requiring shrink <0.1% but little requirement for aesthetics.

Information provided by IDI Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 2.00 g/cc1.80 - 2.00 g/ccASTM D792
Water Absorption 0.10 - 0.30 %
@Time 86400 sec
0.10 - 0.30 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 6030 - 60ASTM D2583
Tensile Strength 41.0 MPa5950 psiASTM D638
Flexural Strength 69.0 MPa10000 psiASTM D790
Compressive Strength 124 MPa18000 psiASTM D695
Izod Impact, Notched 2.13 J/cm3.99 ft-lb/inASTM D256
Izod Impact, Unnotched 4.27 J/cm8.00 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C>= 399 °FASTM D648
Shrinkage 0.00 - 0.0010 %0.00 - 0.0010 %ASTM D955
 
Descriptive Properties
Flammability (Average Burn Rate)1.7 cm/min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIDI927 / 249317

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.