Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
SABIC XENOY™ HX6600HP PC+PBT (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, Gamma and Steam sterilizable.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Density 1.21 g/ccISO 1183
Water Absorption 0.40 %23°C/sat; ISO 62
Moisture Absorption 0.0500 %23°C / 50% RH; ISO 62
Viscosity 210 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.012 - 0.016 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 11 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPa50 mm/min; ASTM D638
 37.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 43.0 MPa50 mm/min; ASTM D638
 44.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ISO 527
 150 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ASTM D638
 4.0 %50 mm/min; ISO 527
Tensile Modulus 1900 MPa5 mm/min; ASTM D638
 1900 MPa1mm/min; ISO 527
Flexural Yield Strength 43.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 64.0 MPa2 mm/min; ISO 178
Flexural Modulus 1800 MPa2 mm/min; ISO 178
 1900 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 800 J/mASTM D256
 750 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 65.0 kJ/m²80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature -40.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 70.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 100 JASTM D3763
Impact Test 100 JMultiaxial Impact; ISO 6603
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 130 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 60.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 117 °CRate B/50; ISO 306
 117 °CRate B/50; ASTM D1525
 120 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 250 - 265 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10841 / 244308

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.