MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sipol Sipolprene® 63210 TPC-ET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyether Ester Elastomer

Material Notes: Description: Sipolprene® 63210 is an ether ester thermoplastic elastomer (TPC-ET), developed and manufactured by Sipol, with a nominal hardness of Shore D 62, a medium modulus, and a rheological behavior, which makes it suitable for injection molding and extrusion processing. Sipolprene® 63210 comes in a natural color with a standard stabilization package, fully in compliance with American FDA and European EU 10/2011 Food Contact Regulations. Black color and/or UV stabilized and/or heat stabilized are all available in dry blend version on request.

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D 792
Water Absorption 0.20 %
@Time 86400 sec
MI 08
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62instantaneous; ASTM D 2240
 59
@Time 15.0 sec
ASTM D 2240
Tensile Strength at Break 50.0 MPaASTM D 638
Elongation at Break 500 %ASTM D 638
Flexural Modulus 300 MPaASTM D 790
Izod Impact, Notched 30.0 J/m
@Temperature -40.0 °C
ASTM D 256
 NB
@Temperature 23.0 °C
ASTM D 256
Tear Strength 210 kN/mASTM D 1004
Taber Abrasion, mg/1000 Cycles 40
@Load 1.00 kg
H-18; ASTM D 1044
 
Thermal PropertiesOriginal ValueComments
Melting Point 211 °CASTM D 3418
Vicat Softening Point 195 °CA/50; ASTM D 1525
Glass Transition Temp, Tg 3.00 °CASTM D 3418
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPOL030 / 297155

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.