MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite SUMILITE® ELC-4762 Glass Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Glass Epoxy Double sided Materials for PCB

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.10 %E-24/50+D-24/23
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 15.0 GPaMD
 15.0 GPaTD
Flexural Strength 470 MPaTD
 539 MPaMD
Flexural Modulus 15.0 GPaTD
 16.0 GPaMD
Peel Strength 1.50 kN/mA; 18umCF
 1.50 kN/mS-20"/260; 18umCF
Film Tensile Strength at Break, MD 260 MPa
Film Tensile Strength at Break, TD 260 MPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.5
@Frequency 1e+9 Hz
C-96/20/65
 4.6
@Frequency 1e+9 Hz
C-96/20/65+D-24/23
 4.7
@Frequency 1e+6 Hz
C-96/20/65
 4.7
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Dissipation Factor 0.014
@Frequency 1e+9 Hz
C-96/20/65
 0.018
@Frequency 1e+6 Hz
C-96/20/65
 0.019
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
 0.020
@Frequency 1e+9 Hz
C-96/20/65+D-24/23
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µin/in-°F10°C/min; Z (a1)
 270 µin/in-°F10°C/min; Z (a2)
CTE, linear, Transverse to Flow 14.0 µin/in-°F10°C/min; X (a1)
 16.0 µin/in-°F10°C/min; Y (a1)
Glass Transition Temp, Tg 135 °C10°C/min
 145 °C20°C/min
 150 °C5°C/min
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite SUMILITE® ELC-4768/EI-6768 Glass Epoxy Laminate
Sumitomo Bakelite SUMILITE® PLC-2147 AQ Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 RF Paper Phenolic
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Sumitomo Bakelite SUMILITE® ELC-4765/EI-6765 Glass Epoxy Laminate

PSUMIT115 / 193920

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.