MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALTECH® PA66 A 2030/310 GF50 Nylon 66, 50% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Base Polymer: Polyamide 66

Filler/Additive System: 50% glass fibers

Special Features: Various

Typical Applications: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psiISO 527
Elongation at Break 3.5 %3.5 %ISO 527
Tensile Modulus 12.0 GPa1740 ksiISO 527
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Charpy Impact Unnotched 8.50 J/cm²40.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection molding
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection molding
Drying Temperature <= 80.0 °C
@Time 7200 - 43200 sec
<= 176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ 90G33 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 14025 Polyamide 66, Heat Stabilized
Asahi Kasei Leona™ 13G50 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 13005 Polyamide 66, General Purpose
Arkema Orgalloy® RS 6630 BLACK Polyamide 6.6 Alloy 30% Glass Fiber reinforced

PALBIS8279 / 242338

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.