Hostacom TRC 352T G22952 is a 20% talc filled PP copolymer, with excellent impact/stiffness balance and good flowability. It is only suitable for painted applications as it contains no UV stabilizer and no scratch resistance package. This grade is delivered in Color G22952. Availability: Europe Application: Automotive Parts; Instrument Panels; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Good Flow; Paintable Information provided by LyondellBasell. |