MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvaloy® 450 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in commercial tubing and fittings. It has a slight tendency to liquate (i.e. separate into high and low melting constituents) if heated slowly through its melting range.

Applications:Braze 450 has found considerable application in pipe brazing in the ship construction industry and for such items as band instruments, brass lamps, aircraft engine oil coolers, plus other situations where a high strength, ductile joint is required. It is a good, general purpose, brazing filler metal for use where a cadmium free filler metal is specified.

Specifications:Braze 450 conforms to the following specifications- AWS A5.8 BAg-5, ASME Boiler & Pressure Vessel Code Sec. II C, SFA-5.8 BAg-5

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.11 g/cc0.329 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 172 - 207 MPa25000 - 30000 psiCopper butt joint
 276 - 345 MPa40000 - 50000 psiBrass butt joint
 310 - 379 MPa45000 - 55000 psiNickel-Silver butt joint
Elongation at Break 13 - 22 %13 - 22 %% in 2", Copper butt joint
 14 - 28 %14 - 28 %% in 2", Nickel-Silver butt joint
 20 - 36 %20 - 36 %% in 2", Brass butt joint
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000908 ohm-cm0.00000908 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 662.8 - 743 °C1225 - 1370 °F
Solidus 662.8 °C1225 °FMelting Point
Liquidus 743 °C1370 °FFlow Point
 
Processing PropertiesMetricEnglishComments
Processing Temperature 743 - 843 °C1370 - 1550 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 29 - 31 %29 - 31 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 44 - 46 %44 - 46 %
Zinc, Zn 23 - 27 %23 - 27 %
 
Descriptive Properties
ColorYellow White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® 560 (Braze™ 560) Silver-Copper-Zinc Alloy (AWS BAg-7)
Lucas-Milhaupt Silvaloy® 401
Lucas-Milhaupt Silvaloy® 452
Lucas-Milhaupt Silvaloy® 541 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal

NLUCMI22 / 18089

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.