GM5010T2B is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. It shows high mechanical properties and has excellent resistance to hydrostatic pressure and to stress cracking. This resin has the MRS (Minimum Required Strength) of 8 MPa, according to ISO 9080, and is classified as PE 80 according to ISO 12162. GM5010T2B is manufactured in a blue color and contains additives to protect it against ultraviolet radiation action and photodegradation. Its applications include blue PE 80 pressure pipes for water branch lines for buildings and distribution and adductors water systems. |