Crystalline ethylene-propylene rubber with medium ENB (ethylidene norbornene) content and a low Mooney viscosity. The high ethylene and low Mooney viscosity contribute to excellent flow properties in combination with a good level of physical properties, very suitable for low-filled, non-black compounds. Typical applications are cable and wire and molded goods for electrical appliances (e.g. connectors)Information provided by Lanxess. |