MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Rogers Arlon E950-10RXX-M8 0.050" (1.27 mm) Cured Silicone Rubber with PSA liner
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: 1 inch wide, 50 mil thick, Red, Rectangular cross-section, Fully cured silicone interleaved with 0.002” PSA liner. Product is supplied in various roll lengths and the xx in the product number indicates roll length in yards.

Design/Construction:
Interleave: Mylar
Pressure Sensitive Adhesive: Silicone
Extrusion: Cured Silicone Rubber
Cross-Section: 1” Wide Rectangular

Arlon STD Certificate of Compliance for commercial applications will be provided with each order.

Appearance: Red silicone rubber on polymer liner

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccTape Property; Arlon SQA-TMS-024
Thickness 2.00 milInterleave
 50.0 milRubber; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52Tape Property; ASTM D2240
Tensile Strength 1096 psiTape Property; ASTM D412
Elongation at Break 358 %Tape Property; ASTM D412
Peel Strength 1.00 pliTape Property; MIL-I-46852C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.1 °C
From date of manufacture
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier
Rogers Arlon 55572XD028 0.028" (0.711 mm) Cured Silicone Rubber
Rogers Arlon 55191R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 55133R062 0.0622" (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate

PARL523 / 125709

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.