MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Solvay MIRACARE® 2 MCAS/E Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Optimized blend of anionic and amphoteric surfactants used in the formulation of low irritation shampoos, skin cleansers and baby care systems. Preserved with Phenonip

C.T.F.A. / I.N.C.I. Name : WATER (AND) DISODIUM COCOAMPHODIACETATE (AND) SODIUM LAURYL SULFATE (AND) SODIUM LAURETH SULFATE (AND) PROPYLENE GLYCOL

CAS: 7732-18-5 / 68650-39-5 / 68585-47-7 / 68585-34-2 / 57 – 55 – 6

EINECS: 231-791-2 / 272-043-5 / 271-557-7 / 500-223-8 / 200 – 338 – 0

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE 2MCAS/E is a blend of amphoteric and anionic surfactants designed to provide optimum mildness and good foam and cleansing performance. Non-irritant formulation base for the preparation of shampoos, baby shampoos, facial washes and shower gels. Mild to skin, non-irritating to eyes. Compatibility with fragrances. Contains Phenonip (blend of Phenoxyethanol, Methylparaben, Ethylparaben, Butylparaben, Propylparaben) as preservative.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 45.5 - 48 %100-water
pH 7.5 - 8.0
@Temperature 30.0 °C
540MA3C1E
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 52 - 54.5 %540MA3C1C
 
Descriptive Properties
AppearanceClear, thin, yellow liquid
CompositionActive Matter30-32%, Solids-NaCl-Propylene glycol
 Phenonip0.001
 Propylene glycol8.5-9.5%
 Sodium Chloride<6.8%, 540MA3C10
 Sodium sulfates<0.7%, 540MA3C17

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Mirasheen® S-188 Surfactant
Solvay MIRACARE® SLB-205/N Surfactant
Solvay MIRACARE® CT-100 Surfactant

WRHOD232 / 137463

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.