MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller U3345 Structural Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: U3345 is a versatile, medium-to-high viscosity UV-curable adhesive that bonds extremely well on a wide variety of substrates. It is suitable for use in a broad spectrum of UV-cure applications, where it provides a tough, flexible bond on plastic, glass and metal.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Brookfield Viscosity 1500 - 2500 cP1500 - 2500 cPRV3
Storage Temperature 8.00 - 21.0 °C46.4 - 69.8 °Fin darkness
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Hardness, Shore D 3232ASTM D2240
Elongation at Break 275 %275 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 95.0 °C>= 203 °F
 
Processing PropertiesMetricEnglishComments
Cure Time <= 0.100 min<= 0.00167 hourSet Time, at 395nm, 50mW/cm2
 1440 min24.0 hourFull Cure Time
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
ColorLight Straw
ConsistencyLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL229 / 317020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.