MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 5775B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B series are highly engineered extrusion-grade thermoplastic vulcanizate with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a medium hardness, medium density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Good Processability; High Heat Resistance; Low Compression Set; Medium Density; Medium Hardness; Resilient

Uses: Automotive Applications; Belts/Belt Repair: Profiles; Rubber Replacement; Seals; Weatherstripping

Agency Ratings: UL 94

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-100 CGV Color: Black; DAIMLER DBL 5562.30 Color: Black; FORD WSS-M2D380-B1; GM QK 3523 L Color: Black; GM Sarlink Color: Black; PSA Peugeot-Citron B62 0300 version G Color: Black; VAG VW501 23 Color: Black

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding; Extrusion; Blow Molding; Profile Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D792
Viscosity 330 cP
@Shear Rate 206 1/s,
Temperature 200 °C
330 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  72
@Time 5.00 sec
72
@Time 0.00139 hour
Extruded; ASTM D2240
 75
@Time 5.00 sec
75
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 7.31 MPa1060 psiFlow; ASTM D412
 8.48 MPa1230 psiAcross Flow; ASTM D412
 7.63 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
1110 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 7.80 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
1130 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  3.20 MPa
@Strain 100 %
464 psi
@Strain 100 %
Across Flow; ISO 37
 4.90 MPa
@Strain 100 %
711 psi
@Strain 100 %
Flow; ISO 37
 3.26 MPa
@Strain 100 %,
Treatment Temp. 150 °C
473 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 3.33 MPa
@Strain 100 %,
Treatment Temp. 135 °C
483 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 340 %340 %Flow; ASTM D412
 590 %590 %Across Flow; ASTM D412
 525 %
@Treatment Temp. 150 °C,
Time 605000 sec
525 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 549 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
549 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 35.1 kN/m200 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  23 %
@Temperature 22.8 °C,
Time 79200 sec
23 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 47 %
@Temperature 125 °C,
Time 252000 sec
47 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Black
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 232 °C360 - 450 °FInjection
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Zone 1 182 - 204 °C360 - 400 °FExtrusion
Zone 2 182 - 204 °C360 - 400 °FExtrusion
Zone 3 188 - 210 °C370 - 410 °FExtrusion
Zone 4 188 - 210 °C370 - 410 °FExtrusion
Die Temperature 193 - 216 °C380 - 420 °FExtrusion
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPV 5765B Thermoplastic Vulcanizate
Teknor Apex Telcar® TL-1445S Thermoplastic Elastomer
Teknor Apex Telcar® OBC 4675A Thermoplastic Elastomer
Teknor Apex Sarlink® TPV 5790B Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV 5755B Thermoplastic Vulcanizate

PTEKNQ1170 / 237661

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.