MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Applications
Petrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with low COF.

Regulatory Status
The basic NA373 resin meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520.

Processing Techniques
Specific recommendations for processing NA373 resins can only be made when the processing conditions, equipment and end use are known.

Key Words: FDA 21 CFR 177.1520.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Thickness 31.8 microns1.25 milCast, as tested
 31.8 microns1.25 milBlown, as tested
Melt Flow 3.0 g/10 min3.0 g/10 minASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 3900 ppm3900 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.38 MPa1360 psiCast; ASTM D822
 10.9 MPa1580 psiBlown; ASTM D822
Film Tensile Strength at Yield, TD 9.31 MPa1350 psiCast; ASTM D822
 10.7 MPa1550 psiBlown; ASTM D822
Film Elongation at Break, MD 200 %200 %Blown; ASTM D822
 230 %230 %Cast; ASTM D822
Film Elongation at Break, TD 500 %500 %Blown; ASTM D822
 610 %610 %Cast; ASTM D822
Elmendorf Tear Strength MD 270 g270 gBlown; ASTM D1922
 300 g300 gCast; ASTM D1922
Elmendorf Tear Strength TD 160 g160 gCast; ASTM D1922
 170 g170 gBlown; ASTM D1922
Dart Drop Test 65.0 g0.143 lbBlown; ASTM D1709, F50
 110 g0.243 lbCast; ASTM D1709, F50
Film Tensile Strength at Break, MD 18.6 MPa2700 psiBlown; ASTM D822
 29.1 MPa4220 psiCast; ASTM D822
Film Tensile Strength at Break, TD 17.0 MPa2470 psiCast; ASTM D822
 17.2 MPa2500 psiBlown; ASTM D822
1% Secant Modulus, MD 159 MPa23000 psiBlown; ASTM D882
 208 MPa30200 psiCast; ASTM D882
1% Secant Modulus, TD 172 MPa25000 psiBlown; ASTM D882
 197 MPa28600 psiCast; ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 3.4 %3.4 %Cast; ASTM D1003
 5.4 %5.4 %Blown; ASTM D1003
Gloss 70 %70 %Blown, 45°; ASTM D2457
 77 %77 %Cast, 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 °C375 °FBlown
 260 °C500 °FCast
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene
Phillips 66 COPYLENE® CM010G Polypropylene Impact Copolymer
Formosa Plastics Formolene® 1102K Cast and BOPP Film Polypropylene
Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene
Formosa Plastics Formolene® 4142N Injection Molding Polypropylene

PEQU0858 / 157479

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.