MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lord Adhesives PCC40533 Silver Conductor
Categories: Polymer; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: LORD PCC40533 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices.

Features: may be applied by screen printing, syringe or pin transfer. provides a working life of 3-5 days in a closed container at room temperature. Working life is reduced to 24 hours (25% increase in viscosity) if material is stored in an open container. rapidly cures between 150-200°C. cured film provides excellent electrical and mechanical properties with good bonding to a variety of substrates.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 7500 - 9500 cP
@Temperature 25.0 °C
7500 - 9500 cP
@Temperature 77.0 °F
Brookfield HBT, Spindle CP-51, 10 rpm
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.000200 ohm-cm
@Treatment Temp. 200 °C,
Time 119 sec
<= 0.000200 ohm-cm
@Treatment Temp. 392 °F,
Time 0.0330 hour
cured on alumina
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature -40.0 °C
6.00 Month
@Temperature -40.0 °F
from date of shipment in original, unopened container
 
Descriptive Properties
AppearanceSilver Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9328 / 232684

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.