MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Meehanite K-295 Austempered Ductile Iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Type K-295 is used for applications such as gears requiring high contact rolling and tooth bending fatigue properties. Type K-295 also possess high fracture toughness impact strength. Excellent founding properties enable more accurate castings with savings in machine stock required. Damping capacity and notch sensitivity are superior to steel castings and forgings. Self-lubricating properties make Type K-405 ideal for wear conditions involving minimal lubrication.

General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.

Information provided by Meehanite Marketing Association.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 280 - 310280 - 310
Tensile Strength, Ultimate 896 MPa130000 psi
Tensile Strength, Yield 676 MPa98000 psi
Elongation at Break 8.0 - 12 %8.0 - 12 %
Fatigue Strength 269 MPa39000 psiEndurance Limit (Notched)
 434 MPa63000 psiEndurance Limit (Unnotched)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium-Silicon Ductile Iron, heat-resistant ductile iron
Meehanite Ductliron® SF-60 Nodular Graphite Ductile Iron
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536
ASTM A897/A897M-06 Grade 750 (110-70-11) Austempered Ductile Iron
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536

NMEE10 / 18231

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.