MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kraiburg TPE For Tec E® OC6OAN Thermoplastic Elastomer (AD/PAX/CR Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The AD/PAX/CR series is used for applications with velvet touch. The material has increased resistance to skin oils, sun cream and olive oil. The compounds are characterized by their adhesion to polyamides, partially aromatic polyamides and polyarylamides. The compounds are available in black and natural colors. Natural color variants can be colored in many different ways.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
  • Black
Typical applications:
  • Function and design elements
  • Soft touch for grips, switches and mats
  • Wearables
  • Ear phones
Material advantages:
  • Adhesion to partially aromatic polyamides (PAX) and polyarylamides (PARA)
  • Adhesion to PA6 and PA6.6, up to 50% glass fiber
  • Adhesion to PA12
  • Resistance to skin oils, sunscreen or olive oil
  • Colorable
  • Non-sticky surface

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060DIN ISO 48-4
Tensile Strength 5.50 MPa798 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 750 %750 %200 mm/min; DIN 53504/ISO 37
Tear Strength 23.5 kN/m134 pliISO 34-1 Method B (b)
 
Descriptive Properties
Adhesion to PARA5.0 N/mm (B/D)VDI 2019 two-component injection
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8425 / 309089

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.