MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Yuyao Zhonga PP-08 PP, 40% Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Typical application: Heat resistance, Mineral filling, Ageing resistance, Good impact, Fan follower, Fan cowl

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inASTM D955
Melt Flow 7.0 g/10 min7.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103DIN 53456
Tensile Strength 41.0 MPa5950 psiASTM D638
Flexural Strength 47.0 MPa6820 psiDIN 53452
Flexural Modulus 2.80 GPa406 ksiASTM D790
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²DIN 53453
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ASTM D256
 
Processing PropertiesMetricEnglishComments
Processing Temperature 195 - 225 °C383 - 437 °FInjection Temp
Mold Temperature 45.0 - 80.0 °C113 - 176 °F
Drying Temperature 90.0 - 95.0 °C194 - 203 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Injection Pressure 60.0 - 90.0 MPa8700 - 13100 psi
 
Descriptive Properties
Ageing Resistance>750 H

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PYUYZ029 / 281822

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.