MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parson Adhesives PARFIX® 3409 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3409 is a gel of ethyl cyanoacrylate adhesive for vertical surfaces.

Applications:

  • Bonding applications for vertical surfaces where adhesive run-off or drip must be avoided.
  • Suitable for wide variety of assembly of Industrial equipment and devices.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 435 - 1310 psiPVC; ASTM D1002
 725 - 1450 psiPolycarbonate; ASTM D1002
 1450 - 2180 psiEtched Aluminum; ASTM D1002
 1450 - 2180 psiNeoprene Rubber; ASTM D1002
 2030 - 3190 psiGrit Blasted Steel; ASTM D1002
 1740 - 3770 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 625 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D696
Thermal Conductivity 0.100 W/m-KASTM C177
Melting Point 160 - 170 °C
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -60.0 °F
Glass Transition Temp, Tg 120 °CASTM E228
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull
 
Descriptive Properties
AppearanceColorless Liquid
Bonding Times15-25 secNeoprene
 15-25 secNitrile Rubber
 20-60 secABS
 20-60 secPolycarbonate
 30-60 secPhenolics
 50-95 secPVC
 50-95 secStainless Steel
 5-30 secAluminum
CompositionEthyl Cyanoacrylate Adhesives
Gap Filling0.5 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN119 / 186562

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.