MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total PPH 3480Z Polypropylene, Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Homopolymer Profile Extrusion Grade

Process Stability --FINA 3480Z is formulated specifically to give excellent process stability in high profile extrusion.

High Purity - Low catalyst residues in FINA 3480Z provide outstanding color, plus low taste and odor.

Antistat - FINA 3480Z is formulated to minimize surface static build-up.

FDA - FINA 3480Z complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 3480Z is recommended for high speed profile extrusion for standard and flexible drinking straws.

Processing - FINA 3480Z processes on conventional extrusion equipment with typical melt temperatures of 390-450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 4.8 g/10 min4.8 g/10 minASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D288A
Hardness, Shore D 7777ASTM D1706
Tensile Strength, Ultimate 35.6 MPa5160 psiASTM D638
Elongation at Break >= 100 %>= 100 %ASTM D638
Elongation at Yield 10 %10 %ASTM D638
Modulus of Elasticity 1.515 GPa219.7 ksiASTM D638
Flexural Modulus 1.38 GPa200 ksiASTM D790
Izod Impact, Notched 0.265 J/cm0.496 ft-lb/inASTM D256A
Izod Impact, Unnotched 12.7 J/cm23.8 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 165 °C329 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 107 °C225 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 232 °C392 - 450 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen HP420M Polypropylene
Total PPH 3429 Polypropylene, Injection Molding Grade
ExxonMobil PP2252E3 Homopolymer
Overview of materials for Polypropylene Copolymer
Total PPH 4030 Polypropylene Homopolymer

PFIN61 / 38391

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.