MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mitsubishi Iupital® FS2022 Copolymer Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Silicone Filled

Material Notes: Low friction and wear resistant 2. Silicone oil contained. Iupital is a copolymer-type acetal resin produced with our proprietary manufacturing process. Used in a wide range of industries, Iupital is ideal for precision machinery, automobile, OA and electronics applications. Well-balanced mechanical properties and high fatigue resistance. Excellent anticreep properties. Excellent low friction and anti-wear properties. Wide range of operating temperatures. High oil and organic chemical resistance. Excellent thermal stability in molding.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Moisture Absorption 0.220 %
@Temperature 23.0 °C
60% RH
Linear Mold Shrinkage, Flow 0.020 cm/cm
@Thickness 3.00 mm
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 56.0 MPaISO-527-1,2
Elongation at Break 51 %ISO 527-1,2
Elongation at Yield 10 %ISO 527-1,2
Tensile Modulus 2700 MPaISO 527-1,2
Flexural Strength 83.0 MPaISO 178
Flexural Modulus 2500 MPaISO 178
Charpy Impact Unnotched 150 kJ/m²ISO 179-1,2
Charpy Impact, Notched 7.50 kJ/m²ISO 179-1,2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-2
Melting Point 166 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75-1,2
Flammability, UL94 HB
@Thickness 0.800 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Powersil® PASTE AP Silicone Paste
RTP Company RTP 800 SI 2 HB Acetal (POM), Silicone Lubricated - UL94 HB
Overview of materials for Acetal Copolymer, Silicone Filled
ITW Devcon® Liquid Release Agent Silicone
Evonik TEGOPREN® 5863 Defoamer

PMITSU9139 / 191812

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.