MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik P84®NT1 15G HCM Aromatic Polyimide, 15% Graphite Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes:
  • Excellent performance at high temperatures
  • High strength and excellent shape stability
  • Very good impact resistance
  • High heat deflection temperature
  • Very good creep resistance even at elevated temperatures
  • Machinable with standard tools
  • Low wear and friction behavior
  • Processing by Hot compression molding
Application examples: bushings, seals, bearings components, guides, gear wheels, and valve parts in the automotive and aerospace industries and in industrial equipment.
Industrial Sector: Automotive and Mobility, Aircraft and Aerospace, Industry and Engineering
Processing: Hot compression molding, Machining
Delivery form: Pellets, Granules, Powder
Resistance to: Heat (thermal stability), Fire / burn, Wear / abrasion, Oil / fuels
Electrical: Insulating
Additives: Lubricant
Applications: Electrical and Electronical, General purpose, Fittings
Processing: Compression molding
Special Characteristics: Halogen-free, PTFE-free, Amorphous, High heat resistant, Non-dripping, Self-extinguishing, Thermally conductive
Features: Creep resistance, Low coefficient of friction, Lightweight
Color: Natural color, Grey
Additives: Conductive agent, Inorganic fillers
Chemical Resistance: Acid resistance, Solvent resistance, Grease resistance, Oil resistance, Radiation resistance, Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183
Water Absorption 0.600 %
@Time 86400 sec
ISO 62
 0.800 %
@Time 173000 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87.0ISO 7619-1
Tensile Strength at Break 103 MPaISO 527
Tensile Strength 103 MPaISO 527
Elongation at Break 6.30 %ISO 527
Tensile Modulus 4000 MPaISO 527
Flexural Strength 152 MPaISO 178
Flexural Modulus 3750 MPaISO 178
Compressive Strength 269 MPaISO 604
Compressive Modulus 4460 MPaISO 604
Charpy Impact Unnotched 45.2 kJ/m²Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 1.50 kJ/m²Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Thermal Conductivity 0.530 W/m-KISO 22007-4
Deflection Temperature at 0.46 MPa (66 psi) 345 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 335 °CISO 75-1/-2
Glass Transition Temp, Tg 357 °CDMA, 3 point bending; ISO 6721-5
 
Descriptive Properties
ColorNatural color, Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7812 / 324944

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.