System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Lehvoss LUVOCOM® 3F PP 9929 NT Polypropylene copolymer for Additive Manufacturing
Categories:
Polymer
;
3D Printing/Additive Manufacturing Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
Material Notes:
Polypropylene-copolymer unreinforced, natural
Main features: Reduced moment of inertia compared with metal parts.
Information provided by Lehmann & Voss & Co.KG
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.900
g/cc
0.900
g/cc
ISO 1183-3
Water Absorption
<= 0.300 %
@Time 86400 sec
<= 0.300 %
@Time 24.0 hour
ISO 62
Melt Flow
8.10
g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.10
g/10 min
@Load 4.76 lb,
Temperature 446 °F
pellet
Mechanical Properties
Metric
English
Comments
Tensile Strength
15.0
MPa
2180
psi
50 mm/min; ISO 527
Elongation at Break
6.00 %
6.00 %
50 mm/min, Fmax; ISO 527
500 %
500 %
50 mm/min; ISO 527
Tensile Modulus
0.750
GPa
109
ksi
1 mm/min; ISO 527
Charpy Impact, Notched
1.00
J/cm²
@Temperature -30.0 °C
4.76
ft-lb/in²
@Temperature -22.0 °F
80x10x4mm; ISO 179 1eA
6.50
J/cm²
@Temperature 23.0 °C
30.9
ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 179 1eA
Electrical Properties
Metric
English
Comments
Surface Resistance
<=
1.00e+12
ohm
<=
1.00e+12
ohm
Ronde 60x4mm; DIN EN 62631-3-2
Insulation Resistance
<=
1.00e+12
ohm
<=
1.00e+12
ohm
strip electrode R25; DIN EN 62631-3-3
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
80.0
°C
176
°F
80x10x4mm; ISO 75
Vicat Softening Point
135
°C
275
°F
VST A; DIN ISO 306
Processing Properties
Metric
English
Comments
Nozzle Temperature
220
-
250
°C
428
-
482
°F
Zone 1
220
-
250
°C
428
-
482
°F
Zone 2
220
-
250
°C
428
-
482
°F
Zone 3
230
-
260
°C
446
-
500
°F
Melt Temperature
60.0
°C
140
°F
Mold Temperature
40.0
-
80.0
°C
104
-
176
°F
Drying Temperature
70.0
-
95.0
°C
@Time 7200 - 14400 sec
158
-
203
°F
@Time 2.00 - 4.00 hour
Dehumidifying
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLUU8736 / 325120
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.