Function: Activated semi-ultra accelerator for the vulcanization of natural and synthetic rubbers; excellent dispersion of MBTS, even in soft compounds Application: Technical rubber articles of all kinds; soft compounds, sponge rubber, delicate technical rubber components where dispersion is decisive for the technical performance and lawless functioning. Information provided by Lanxess. |