MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NIZHNEKAMSKNEFTEKHIM PP 4340S (EP2H49G) Propylene and Ethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polypropylene (PP)

Material Notes: Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited, effective nucleation, improved optical properties, improved antistatic properties to produce articles, and improved rheology of melt.

Information provided by manufacturer

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 38 - 46 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238/L
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus >= 950 MPaASTM D790
Izod Impact, Notched >= 45.0 J/mASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 137777 C Polypropylene (PP) Copolymer - High Flow - High Impact - Flame Retardant - UV Stabilized
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength
Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
NIZHNEKAMSKNEFTEKHIM PP 8348S (EPH31RA) Propylene and Ethylene Block Polymer

PNKNH038 / 109305

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.