MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay MIRASHEEN® CP-820/G Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related products to impart opacity and pearlescence.

Identification: COCAMIDOPROPYL BETAINE, GLYCOL DISTEARATE, LAURETH-7, SODIUM COCOAMPHOACETATE, SODIUM LAURETH SULPHATE, WATER

CAS: 70851-07-9 , 627-83-8 , 68002-97-1 , 68608-65-1 , 91648-56-5, 7732-18-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Usage of MIRASHEEN CP-820/G at 1.0 to 5.0% provides a superior pearlescent effect. The concentrate can be incorporated by mixing it with the base formulation at ambient temperatures followed by pH and viscosity adjustments as required. Slow blending of MIRASHEEN CP-820/G into the formulation with smooth agitation results in a finished product exhibiting excellent pearlescence and stability. MIRASHEEN CP-820/G is also suitable for use over a broad pH range. MIRASHEEN CP-820/G are ready to use liquid pearlising concentrates that deliver excellent pearlescence, as well as distinct emolliency, mildness and moisturising benefits to the skin. In addition, they also contain ingredients that provide viscosity building, foam stability and lather enhancement characteristics. Thanks to the amphoteric and non-ionic components, MIRASHEEN CP series is compatible with all surfactants types. Their unique composition contributes to significant wet-combout. Mild baby-type products and other high foaming Personal Care products may be easily formulated using this cold pearliser, since the ingredients in this concentrate are commonly found in these types of products.

Information provided by Rhodia, Rhodia has been acquired by Solvay. The Mirasheen® brand has been sold to Verdant Specialty Solutions, although this specific grade has been discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 33 - 38 %
@Temperature 110 °C,
Time 3600 sec
33 - 38 %
@Temperature 230 °F,
Time 1.00 hour
RP-0540
pH 6.0 - 8.06.0 - 8.010% Aqueous; RP-0420
Brookfield Viscosity <= 10000 cP<= 10000 cP#3 sp @ 12 rpm; RP-0596
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearancePearlescent flowable pasteRP-0064

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD277 / 137508

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.