MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Accella Bayblock® Primer RI Primer
Categories: Polymer

Material Notes: Bayblock Prime RI is a water-based two component rust inhibitive primer.

Properties / Applications: Bayblock Prime NS is designed for the preparation of surfaces for the application of elastomeric coatings and spray polyurethane foam. This material can be easily sprayed, rolled, or brushed on and provides excellent adhesion to most surfaces. Bayblock Prime NS primer requires minimal set time before foam application. This product is water reducible. Use of Bayblock Prime NS primer in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³
Solids Content 58 - 62 %58 - 62 %by volume
 60 - 64 %60 - 64 %by weight
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ASTM D2240
Impact Test >= 18.1 J>= 13.3 ft-lbASTM D2794
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air 10.0 °C50.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 240 min240 min
 
Descriptive Properties
ColorOrange

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0065 / 201848

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.