MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis HE4883 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HE4883 is a fully formulated Azodicarbonamide free compound for physical foamed data cable insulation. HE4883 is a high-density polyethylene compound containing blowing agent for the production of foam or foam-skin insulation.

Typical characteristics:

  • Optimal cell structure
  • High process control
  • Smooth surface
  • Improved crushability
  • Easy extrusion ADCA-free
Applications:
  • Data cables
Specifications: HE4883 is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures.
  • ASTM D1248 Type III, Class A, Category 3, Grade E1, E3
  • EN 50290-2-33

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.600 g/cc
Density 0.949 g/ccISO 1183-1
Melt Flow 3.50 g/10 min
@Load 5.00 kg,
Temperature 140 °C
ISO 1133-1
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61.0
@Time 1.00 sec
ISO 868
Tensile Strength 23.0 MPa25 mm/min; ISO 527-2
Elongation at Break 600 %25 mm/min; ISO 527-2
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.29
@Frequency 1.90e+9 Hz
IEC 60250
 2.33
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0000900
@Frequency 1e+6 Hz
IEC 60250
 0.000175
@Frequency 1.90e+9 Hz
IEC 60250
 
Processing PropertiesOriginal ValueComments
Processing Temperature 210 °CFlange
Zone 1 160 °C
Zone 2 190 °C
Zone 3 210 °C
Zone 4 210 °CGas Injection Zone
Zone 5 210 °C
Adapter Temperature 210 °C
Die Temperature 220 °C
Head Temperature 210 °C
Shelf Life 18.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9793 / 323150

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.