MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Tecnoflon® L 636 Fluorelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: TECNOFLON® L 636 is a medium-low viscosity fluoroelastomer terpolymer with 66% fluorine content, designed to provide improved low temperature characteristics. Tecnoflon® L 636 does not contain curatives: therefore the proper levels of Tecnoflon® FOR M1 and Tecnoflon® FOR M2 must be added to achieve the required properties. Tecnoflon® L 636 is especially suited for injection molding of O-rings and sealing components which must meet demanding specifications. Tecnoflon® L 636 exhibits the same excellent heat and chemical resistance expected from Tecnoflon® copolymers.

Some of the basic properties of TECNOFLON® L 636 are:
- Improved low temperature performance
- Good heat and chemical resistance
- Very low compression set
- Excellent mold release
- Lack of mold fouling
- Superior mold flow

Tecnoflon® L 636 can be used for compression, injection and transfer molding of O-rings, diaphragms, gaskets, seals, molded shapes or other items requiring improved low temperature performance. Tecnoflon® L 636 can be combined with the cure system and other typical fluoroelastomer compounding ingredients. Mixing can be accomplished with two-roll mills or internal mixers. This material can be extruded into hoses or profiles and can be calendered to make sheet stocks or belting.
Finished goods can be produced by a variety of rubber processing methods.

Applications: Belts/Belt Repair; Blending; Diaphragms; Gaskets; Hose; Low Temperature Applications; Profiles; Seals; Sheet

Features: Chemical Resistant; Good Flow; Good Mold Release; High Heat Resistance; Low Compression Set; Medium-low Viscosity; Terpolymer

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 35
@Temperature 121 °C
ML 1+10; ASTM D1646
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %
 
Descriptive Properties
AvailabilityEurope
 North America
ColorTranslucent
FormsSlab
ProcessingCalendering; Compounding; Compression Molding; Extrusion
 Injection Molding; Resin Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4517 / 280317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.