MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro DESMOPHEN® NH XP 2701 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Desmophen NH XP 2701 resin is a solvent-free, amine functional reactive partner for polyisocyanates.

Properties / Applications: Desmophen NH XP 2701 resin is a low viscosity amine functional resin developed for use in the formulation of high solids two-component polyurethane/urea coatings. This resin provides faster final cure properties as well as higher coating hardness when compared to other Desmophen NH types. Desmophen NH XP 2701 resin may be used by itself or as a blend with hydroxy-functional acrylic resins and crosslinked with an aliphatic polyisocyanate to yield high solids polyurethane/urea coatings. Desmophen NH XP 2701 resin may also be blended with other amine functional resins, e.g. Desmophen NH 1520, Desmophen NH 1220 in order to obtain customized potlife/dry time characteristics. As with any product, use of Desmophen NH XP 2701 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Viscosity 1100 - 2200 cP
 
Descriptive Properties
Color<250Hazen
Content199-205 mg KOH/gAmine Value

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0754 / 202537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.