For geological prospecting, coal mining, tipping of electric and air drilk; for coal bed and other homogeneous rocks such as non-silicified shale, skyline and rock salt, etc.; and for medium hard sandstone limestone and interspersed soft and hard rocks.Information provided by China Tungsten |