MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMT Materials REN Shape® 5169 Foundry Pattern Board
Categories: Polymer

Material Notes: REN SHAPE 5169 is an extremely tough, abrasion resistant board for use in CNC-machining foundry patterns, core boxes and other tools. It can be milled with hardened-steel cutters. The material has found extensive use in the fabrication of prototype molds for clear, thin-gage thermoplastic sheets. Resultant parts show excellent transparency results. REN SHAPE 5169 features these unique qualities:

  • Excellent Impact and Wear Resistance
  • Superior Edge Definition and Dimensional Stability
  • Polishable to a High Luster
  • Good Compressive and Tensile Strength
  • Tough and Resilient

Applications: REN SHAPE 5169 applications may include prototype thermoforming molds, prototype and production foundry patters, tooling aids and fixtures, and metal forming tools.

Information Provided by CMT Materials, Inc.

Key Words: Renshape
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 75.0 lb/ft³ASTM D-792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D-2240
Tensile Strength, Ultimate 9000 psiASTM D-638
Flexural Strength 14000 psiASTM D-790
Flexural Modulus 380 ksiASTM D-790
Compressive Strength 8800 psiASTM D-695
Compressive Modulus 366 ksiASTM D-695
Izod Impact, Notched 0.900 ft-lb/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.8 µin/in-°F
@Temperature -30.0 - 30.0 °C
ASTM D-3386
Glass Transition Temp, Tg 206 °FASTM D-4065
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hard Foundry Type Alloy (UNS L53710)
Reade Advanced Materials Bentonite Powder (BaTiSi3O9)
Hard Foundry Type Alloy (UNS L53780)
Bohler-Uddeholm UDDEHOLM Carmo Granshots Tool Steel Foundry Meltstock
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Sand Cast

PCMT019 / 93154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.