MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Nemcon™ E PK DP104 is a carbon fiber reinforced polyetheretherketone, characterized by high strength, stiffness, consistent moldabiliity, and exceptional thermal resistance.

All properties after 48hrs conditioning at 23°C/50% RH

Key Words: PEEK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPa50 mm/min; ASTM D638
Elongation at Break 2.0 %50 mm/min; ASTM D638
Tensile Modulus 19540 MPa50 mm/min; ASTM D638
Flexural Strength 320 MPa1.3 mm/min; ASTM D790
Flexural Modulus 18.6 GPa1.3 mm/min; ASTM D790
Izod Impact, Notched 1.65 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 332 °C
@Thickness 3.20 mm
Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate
Ovation Polymers Nemcon™ H PA DP117/X3 Polyphthalamide, Thermally Conductive
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK
Ovation Polymers Nima™ NH PC143P Polycarbonate
Ovation Polymers OpteSTAT™ NC PK 8010 Polyetheretherketone based Carbon Nanotube Compound

POVAT137 / 79116

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.