MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

PSM Industries Pacific Sintered Metals FP-1650-S Phosphorous Iron Soft Magnetic Powdered Metal
Categories: Metal; Ferrous Metal

Material Notes: For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.

All information provided by Pacific Sintered Metals.

Key Words: PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.00 - 7.20 g/cc0.253 - 0.260 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 353 MPa51200 psi
Elongation at Break 12 %12 %
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 3.7<= 3.7K-Gauss/Oe
Magnetic Coercive Force, Hc 1.2 Oe1.2 Oe
Magnetic Saturation Flux Density, Bmax 12700 Gauss12700 GaussMagnetic Induction
Magnetic Remanence, Br 10100 Gauss10100 Gauss

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NPACIF047 / 86205

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.